Design essentials of injection molding parts

Release time:2024-04-09

stayInjection moldingIn the process, due to the uneven cooling and shrinkage of plastic in the mold cavity and the unreasonable structural design of injection molded parts, it is easy to cause various defects of products: shrinkage, weld marks, pores, deformation, galling, top injury, flash.


In order to obtain high-quality injection molded products, the structural manufacturability of products must be fully considered in the design. Next, combined with the main structural characteristics of injection molding products, the methods to avoid injection molding defects are analyzed.

圖片6.png


1、 Mold opening direction and parting line

At the beginning of each injection product design, the mold opening direction and parting line should be determined first, so as to minimize the influence of the core pulling mechanism and the parting line on the appearance. So pay attention to the key points.

1. After the mold opening direction is determined, the stiffener, buckle, bulge and other structures of the product should be designed to be consistent with the mold opening direction as far as possible, so as to avoid core pulling, reduce the suture, and extend the service life of the mold.

2. For example, the mold opening direction of the bumper is generally the body coordinates χ If the mold opening direction is designed as χ If the shafts are inconsistent, the included angle must be indicated in the product drawing.

3. After the mold opening direction is determined, the appropriate parting line can be selected to improve the appearance and performance.


2、 Demoulding slope

1. Proper demoulding slope can avoid product galling. The demoulding slope of smooth surface should be greater than 0.5 degrees, that of fine grained surface should be greater than 1 degree, and that of coarse grained surface should be greater than 1.5 degrees.

2. Proper demoulding slope can avoid damage to the top of the product.

3. When designing products with deep cavity structure, the slope of the outer surface should be less than that of the inner surface, so as to ensure that the mold core does not shift during injection molding, obtain uniform product wall thickness, and ensure the material density and strength of the opening of the product.


3、 Product wall thickness

1. All kinds of plastics have a certain wall thickness range, generally 0.5~4mm. When the wall thickness exceeds 4mm, it will cause problems such as too long cooling time and printing. We should consider changing the structure of the product.

2. Uneven wall thickness will lead to surface reduction.

3. Uneven wall thickness will cause pores and weld marks.


4、 Stiffener

1. Reasonable application of stiffeners can increase the rigidity of products and reduce deformation.

2. The thickness of the stiffener must be less than 1/3 of the product wall thickness, otherwise the surface will be reduced.

Copyright: Shenzhen Zhongyuan Plastic Co., Ltd. | mold processing customized manufacturer. If you want to know the processing price of the factory, how much is it, and which is good, please contact us Yue ICP Bei No. 17060480
久久99精品国产麻豆不卡| 久久久精品视频免费在线| 蜜臀av性久久久久蜜臀| 国模无码视频一区二区三区| 蜜臀AV久久精品人人槡| 内精品自线自拍1717| 国产四级片免费久久久久久| 国产成人精品久久亚洲高清| 两性色午夜视频国产情侣| 久久久一区二区三区毛片| 亚洲最大综合丁香五月天| 国产69精久久久九九九| 久久www成人免费观看| 午夜大胆裸体A级人体片| 亚洲欧美日韩乱码中文字| J国产精品无码久久综合| 日韩欧美一区二区精品视频| Av大片在线不卡免费看| 久久久综国产合九色综合| 三级国产短视频在线观看| 伊人久久大香线蕉AⅤ色| 亚洲午夜av一区二区三区| 亚洲熟悉妇女xxx妇女av| 8AV国产精品爽爽ⅤA在线观看| 日韩欧美国产偷亚洲清高| 久久精品熟女亚洲av麻豆| 自慰高潮喷白浆在线观看| 中文字幕亚洲欧美国产一区 | 久久夜色精品亚洲艾草网| 国产美女 91 在线播放| 久久精品亚洲中文字幕无码网站| 午夜av在线一区二区三区| 久久久久有精品国产免费| 欧美 日韩图片一区二区| 妺妺窝人体色www在线小说| 国内综合精品一区二区av| 性久久久久久| 成人区精品一区二区不卡| 日韩精品制服诱惑中文字幕| 亚洲av无码成人精品国产| 亚洲国产精品热久久|